[1] CUI Kai,LI Yongkui.Fabrication,mechanical properties and thermal shock resistance of laminated TiB2-based ceramic[J].International Journal of Refractory Metals and Hard Materials,2016(54):148-153. [2] CLEGG W J,KENDALL K ,ALFORD N M,et al.A simple way to make tough ceramics[J].Nature,1990,347(4):455-457. [3] LI Yuanyuan,LI Qinggang,WANG Zhi.Microstructures and mechanical properties of laminated ZrC-SiC composites with different SiC powders[J].Ceramics International,2015,41(10):15255-15260. [4] WEI Chuncheng,ZHANG Xinghong,LI Shuang.Laminated ZrB2-SiC/graphite ceramics with simultaneously improved flexural strength and fracture toughness[J].Ceramics International,2014(40):5001-5006. [5] LI Yuanyuan,LI Qinggang,WANG Zhi,et al.Oxidation behavior of laminated ZrB2-SiC composites and monolithic ZrB2-SiC composites[J].Ceramics International,2016,42(1):2063-2069. [6] 申良机,李文新,张莉.碳化硼陶瓷烧结方法的分析研究[J].哈尔滨商业大学学报(自然科学版),2010,26(5):608-618. [7] ZHANG Fenggang,ZHU Xiaopeng,LEI Mingkai.Tribological behavior of WC-Ni cemented carbide irradiated by high-intensity pulsed ion beam[J].Surface & Coatings Technology,2014(258):78-85. [8] TYLER L Stewart,KEVIN P Plucknett.The sliding wear of TiC and Ti(C,N) cermets prepared with a stoichiometric Ni3Al binder[J].Wear,2014,318(1/2):153-167. [9] SHON In-Jin,JEONG In-Kyoon,KO In-Yong,et al.Sintering behavior and mechanical properties of WC-10Co,WC-10Ni and WC-10Fe hard materials produced by high-frequency induction heated sintering[J].Ceramics International,2009,35(1):339-344. [10] GUO Zhixing,XIONG Ji,YANG Mei,et al.WC-TiC-Ni cemented carbide with enhanced properties[J].Journal of Alloys and Compounds,2008,465(1/2):157-162. [11] 田育.现代机械制造业中的刀具失效形式分析[J].价值工程,2011,30(26). [12] 金宏平,陈建国,王志光.切削参数对304奥氏体不锈钢加工表面性能的影响[J].汽车科技,2013(1):66-69. [13] 肖琪聃,吕振林,张珊珊,等.不同压力下Ti3SiC2陶瓷的干摩擦磨损性能研究[J].西安交通大学学报,2011,45(2):121-124. [14] 黄雪红,季德生,赵军.Inconel718与硬质合金摩擦磨损特性的实验研究[J].润滑与密封,2011,36(3):89-93. |